(6) Elutriation separation of the product from chromite reduction at 1500 °C in the presence of SPL demonstrated its effectiveness in upgrading the ferrochrome alloy particles into a concentrate containing 53.0 wt.% Cr and 28.5 wt.% Fe, with a 68.4 wt.% recovery of Cr and Fe, while most slag components were effectively rejected.